7475 Aluminum Plate & Sheet

Arch Metals supplies 7475 aluminum plate and sheet from Dallas, Texas, for aerospace and defense manufacturers across Texas and the surrounding states. 7475 is a high-purity, high-strength alloy known for excellent fracture toughness. We supply it mainly as 7475-T7351 plate and 7475-T7651 plate and sheet, with certified material and saw cutting to your dimensions. Availability depends on temper and thickness, so request a quote and we’ll confirm what we can supply.

7475 Aluminum Plate and Sheet Forms

  • Plate, saw cut to size
  • Sheet
  • Cut blanks and strips on request

Thickness, diameter and length availability changes with mill supply. Send us your sizes through our quote request form and we’ll confirm stock, lead time and pricing.

Aluminum flat bars, representative of 7475 aluminum stock

7475 Aluminum Tempers and Specifications

  • 7475-T7351 plate (AMS 4202, ASTM B209): solution heat treated, stretched and overaged for the best combination of toughness and stress-corrosion resistance.
  • 7475-T7651 plate and sheet (AMS 4085 sheet, ASTM B209): a less fully overaged temper with higher strength and good exfoliation resistance.

Not sure which temper or specification your drawing calls for? Send us the print requirements and we’ll match the material.

Typical Properties of 7475-T7351 Aluminum

  • Ultimate tensile strength: about 72 ksi (496 MPa)
  • Yield strength: about 63 ksi (434 MPa)
  • Elongation: about 13%
  • Density: 0.101 lb/in³ (2.80 g/cm³)
  • Chemistry: aluminum alloyed with zinc, magnesium, copper and chromium, with tightly limited iron and silicon

These are typical values for 7475-T7351 plate. Guaranteed minimums vary by specification, temper and thickness, so check the governing spec or your mill cert for design values.

Why Engineers Choose 7475 Aluminum

7475 is a controlled-purity version of 7075 aluminum. Tighter limits on iron and silicon give it some of the highest fracture toughness of any high-strength aluminum alloy, along with strong resistance to fatigue crack growth. That makes it a common choice for damage-tolerant aircraft structure. For thick-section parts, see 7050 aluminum plate. Common uses for 7475 include:

  • Fuselage and wing skins
  • Bulkheads and pressure-cabin structure
  • Damage-tolerant aircraft structural parts
  • Space and defense structures
Stacked aluminum round bars at a metals service center

7475 Aluminum FAQs

What is the difference between 7475 and 7075 aluminum?

7475 is a controlled-purity version of 7075. Lower iron and silicon content gives it much higher fracture toughness and better fatigue performance at similar strength.

Which 7475 temper should I choose?

T7351 gives the best stress-corrosion resistance and toughness. T7651 gives higher strength with good exfoliation resistance. Your drawing or customer specification will usually name the temper.

Do you supply other aerospace plate alloys?

Yes. We also supply 7050 plate and 2124 plate for thick-section parts.

Cut-to-Size 7475 Aluminum With Delivery Across Texas

We ship 7475 aluminum plate and sheet throughout Texas, Oklahoma, Louisiana, New Mexico and Arizona, and we saw plate to the size you need. See our processing services for cutting options, or browse all the metals we supply.

To get pricing, send us the alloy, temper, form, size, length and quantity through our quote request form, or call (888) 444-6061.